MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Osterman & Co Osterlene® HD600-GP HDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Product Description: HD600-GP is a copolymer with a narrow molecular weight distribution. It provides high impact strength, excellent color, low odor and good processing stability. Typical applications for HD600-GP include open head pails and large shipping containers.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America
Features: Copolymer; Good Colorability; Good Processing Stability; High Density; High Impact Resistance; Low Odor; Narrow Molecular Weight Distribution
Uses: Pails; Shipping Containers
Processing Method: Injection Molding

Information provided by Osterman & Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.953 g/ccASTM D792
Melt Flow 6.9 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 71ASTM D2240
Tensile Strength at Break 3100 psiASTM D638
Tensile Strength, Yield 4130 psiASTM D638
Elongation at Break 1200 %ASTM D638
Elongation at Yield 9.0 %ASTM D638
Flexural Modulus 205000 psiASTM D790
1% Secant Modulus 119000 psiTensile; ASTM D638
 192000 psiFlexural; ASTM D790
2% Secant Modulus 158000 psiFlexural; ASTM D790
Izod Impact, Notched 0.730 ft-lb/inASTM D256
Izod Impact, Unnotched NBASTM D4812
 
Thermal PropertiesOriginal ValueComments
Melting Point 267 °FASTM D3418
Crystallization Temperature 242 °FPeak; ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 164 °FUnannealed; ASTM D648
Vicat Softening Point 262 °FASTM D1525
Brittleness Temperature <= -105 °FF50; ASTM D746

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

POSTER042 / 267624

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.