MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Oxygen-free silver-bearing Copper, UNS C10400, H04 Temper, Rod
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: Hard

Fabrication Properties: Excellent Suitability – Soldering, Brazing, Capacity for Being Cold Worked, Capacity for Being Hot Formed; Good Suitability – Gas Shielded Arc Welding, Butt Weld; Fair Suitability – Oxyacetylene Welding

Common Fabrication Processes: Blanking, Coining, Coppersmithing, Drawing, Etching, Forming and Bending, Heading and Upsetting, Hot Forging and Pressing, Piercing and Punching, Roll Threading and Knurling, Shearing, Spinning, Squeezing and Swaging, Stamping

Typical uses: Gaskets; Radiators; Busbars; Commutator Segments; Conductivity Wire; Contacts; Printed Circuit Foil; Radio Parts; Switches; Terminal Connectors; Windings; Applications Requiring Brazing in Hydrogen Atmosphere; Chemical Process Equipment; Clad Metals; Heat Exchangers; Printing Rolls

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.94 g/cc0.323 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B  45
@Thickness 25.4 mm
45
@Thickness 1.00 in
 47
@Thickness 50.8 mm
47
@Thickness 2.00 in
 60
@Thickness 6.35 mm
60
@Thickness 0.250 in
Hardness, Rockwell F  85
@Thickness 25.4 mm
85
@Thickness 1.00 in
 87
@Thickness 50.8 mm
87
@Thickness 2.00 in
 94
@Thickness 6.35 mm
94
@Thickness 0.250 in
Tensile Strength  310 MPa
@Thickness 50.8 mm
45000 psi
@Thickness 2.00 in
 331 MPa
@Thickness 25.4 mm
48000 psi
@Thickness 1.00 in
 379 MPa
@Thickness 6.35 mm
55000 psi
@Thickness 0.250 in
Tensile Strength, Yield  276 MPa
@Thickness 50.8 mm
40000 psi
@Thickness 2.00 in
0.5% Ext
 303 MPa
@Thickness 25.4 mm
44000 psi
@Thickness 1.00 in
0.5% Ext
 345 MPa
@Thickness 6.35 mm
50000 psi
@Thickness 0.250 in
0.5% Ext
Elongation at Break 10 %10 %
 16 %16 %
 20 %20 %
Tensile Modulus 117 GPa17000 ksi
Modulus of Rigidity 44.1 GPa6400 ksi
Poissons Ratio 0.330.33Calculated
Machinability 20 %20 %
Forgeability 65 %65 %
Shear Strength  179 MPa
@Thickness 50.8 mm
26000 psi
@Thickness 2.00 in
 186 MPa
@Thickness 25.4 mm
27000 psi
@Thickness 1.00 in
 200 MPa
@Thickness 6.35 mm
29000 psi
@Thickness 0.250 in
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000172 ohm-cm0.00000172 ohm-cm100% IACS
 
Thermal PropertiesMetricEnglishComments
CTE, linear  16.9 µm/m-°C
@Temperature 20.0 - 100 °C
9.40 µin/in-°F
@Temperature 68.0 - 212 °F
 17.3 µm/m-°C
@Temperature 20.0 - 200 °C
9.60 µin/in-°F
@Temperature 68.0 - 392 °F
 17.6 µm/m-°C
@Temperature 20.0 - 300 °C
9.80 µin/in-°F
@Temperature 68.0 - 572 °F
Thermal Conductivity 32.3 W/m-K224 BTU-in/hr-ft²-°F
Melting Point 1083 °C1981 °F
Annealing Point 482 - 760 °C900 - 1400 °F
 
Processing PropertiesMetricEnglishComments
Hot-Working Temperature 760 - 871 °C1400 - 1600 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu >= 99.95 %>= 99.95 %
Oxygen, O <= 0.0010 %<= 0.0010 %
Silver, Ag >= 0.027 %>= 0.027 %
 
Descriptive Properties
Cold Work (%)162 in
 351 in
 400.25 in
US EPA Registered AntimicrobialYes

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

MC10400x2 / 292663

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.