MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

ConocoPhillips Hydroclear® 5W-20 Super All Season and Super Motor Oil
Categories: Fluid; Lubricant

Material Notes: Description: Conoco Hydroclear Super All Season Motor Oil SAE 5W-20 is a premium-quality passenger car motor oil developed to meet the requirements of newer, low-friction gasoline engines designed to operate on low viscosity engine oils. It is designed to meet year-round requirements of many 2001 and newer vehicles. Consult Owner Guide for specific application. Hydroclear Super All Season Motor Oil SAE 5W-20 outperforms and outprotects conventional solvent-refined motor oils. It delivers synthetic performance at both very low and very high operating temperatures. Hydroclear Super All Season Motor Oil SAE 5W-20 is formulated with premium base stocks and advanced chemistry to minimize engine deposits and wear, protect against high-temperature oxidation, low-temperature gelling, rust and corrosion and foaming. The friction reducing components in this motor oil provides superior energy-conserving characteristics which result in measurable improvement in fuel economy, when compared to SAE 5W-30 and 10W-30 motor oils. Hydroclear Super All Season Motor Oil SAE 5W-20 meets the performance requirements of ILSAC GF-3 and API SL and is specially formulated for Ford, Honda and other vehicles recommending SAE 5W-20 motor oil.

Information provided by ConocoPhillips.

Phillips 66 Lubricants was spun-off from ConocoPhillips in 2012, and branding was further reorganized in 2016. The Hydroclear® trade name is no longer in use but products may be available under different names.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
API Gravity 37 °37 °
Viscosity  5900 cP
@Temperature -30.0 °C
5900 cP
@Temperature -22.0 °F
Cold-Cranking Viscosity
 18000 cP
@Temperature -35.0 °C
18000 cP
@Temperature -31.0 °F
MRV TP-1
Viscosity Measurement 147147Viscosity Index
Saybolt Viscosity at 100°F 225 SUS225 SUS
Saybolt Viscosity at 210°F 55 SUS55 SUS
Kinematic Viscosity at 40°C (104°F) 50 cSt50 cSt
Kinematic Viscosity at 100°C (212°F) 8.5 cSt8.5 cSt
ASTM Color 3.53.5
 
Thermal PropertiesMetricEnglishComments
Pour Point -45.0 °C-49.0 °F
Flash Point 224 °C435 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WCON036 / 75073

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.