MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

RESPOL REPSOL PRIMEVA® P1807C EVA
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate; Molded/Extruded

Material Notes: Product Description: EVA copolymer REPSOL PRIMEVA® P1807C is suitable for extrusion applications (sheets, profiles, pipes). This material combines easy processability with excellent mechanical properties. It contains antioxidant additives.
Applications: Extrusion - Sheets, Pipes, Profiles
Recommended melt temperature below 200°C to avoid the decomposition of the polymer. Processing conditions should be optimized for each production line.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Additive: Antioxidant

Features: Antioxidant; Copolymer; Food Contact Acceptable; Good Processability

Uses: Piping; Profiles; Sheet

Agency Ratings: EU Food Contact

Processing Method: Extrusion

Information provided by REPSOL

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.941 g/cc0.0340 lb/in³ISO 1183
Vinyl Acetate Content 18 %18 %
Melt Flow 0.70 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.70 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 800 %
@Thickness 0.102 mm
800 %
@Thickness 0.00400 in
ISO 527-3
Film Elongation at Break, TD 900 %
@Thickness 0.102 mm
900 %
@Thickness 0.00400 in
ISO 527-3
Elmendorf Tear Strength MD 245 g
@Thickness 0.102 mm
245 g
@Thickness 0.00400 in
ISO 6383-2
Elmendorf Tear Strength TD 345 g
@Thickness 0.102 mm
345 g
@Thickness 0.00400 in
ISO 6383-2
Dart Drop Test >= 1400 g
@Thickness 0.102 mm
>= 3.09 lb
@Thickness 0.00400 in
F50; ISO 7765-1
Film Tensile Strength at Break, MD 31.0 MPa
@Thickness 0.102 mm
4500 psi
@Thickness 0.00400 in
ISO 527-3
Film Tensile Strength at Break, TD 32.0 MPa
@Thickness 0.102 mm
4640 psi
@Thickness 0.00400 in
ISO 527-3
 
Thermal PropertiesMetricEnglishComments
Melting Point 87.2 °C189 °F
Vicat Softening Point 62.2 °C144 °FISO 306/A
 
Optical PropertiesMetricEnglishComments
Haze 4.0 %4.0 %ASTM D1003
 
Processing PropertiesMetricEnglishComments
Melt Temperature 200 °C392 °F
Blow-up Ratio (BUR) 2.52.5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PRESPOL1319 / 312012

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.