MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Plaskolite Optix® DA Digital Acrylic Sheet
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, Optical Sheet

Material Notes: Designed to provide optimal adhesion of UV curing inks without adhesion promoters, OPTIX DA is a continuously processed acrylic sheet specially formulated product for printing. OPTIX DA provides superior strength and is available in a variety of sizes and thicknesses.

Data provided by the manufacturer, Plaskolite, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.19 g/cc0.0430 lb/in³ASTM D792
Water Absorption 0.40 %0.40 %ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 9595ASTM D785
Tensile Strength 76.05 MPa11030 psiASTM D638
Elongation at Break 5.8 %5.8 %ASTM D638
Tensile Modulus 3.38 GPa490 ksiASTM D638
Flexural Strength 117 MPa17000 psiASTM D790
Flexural Modulus 3.38 GPa490 ksiASTM D790
Izod Impact, Notched 0.149 J/cm0.280 ft-lb/inMilled Notch; ASTM D256
 0.214 J/cm0.400 ft-lb/inMolded Notch; ASTM D256
Tensile Impact Strength 42.0 kJ/m²20.0 ft-lb/in²ASTM D1822
 
Thermal PropertiesMetricEnglishComments
CTE, linear 54.0 µm/m-°C
@Temperature -34.4 - -1.11 °C
30.0 µin/in-°F
@Temperature -30.0 - 30.0 °F
ASTM D696
Thermal Conductivity 0.130 W/m-K0.900 BTU-in/hr-ft²-°FASTM C177
Melting Point 149 - 157 °C300 - 315 °F
Maximum Service Temperature, Air 76.7 - 87.8 °C170 - 190 °FContinuous
Deflection Temperature at 0.46 MPa (66 psi) 97.2 °C207 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C203 °FASTM D648
Softening Point 98.9 - 104 °C210 - 220 °F
Flame Spread 25.88 mm/min1.019 in/minASTM D635
Flame Spread Index 115115ASTM E84
Ignition Temperature 445 °C833 °FSelf Ignition; ASTM D1929
Shrinkage <= 5.0 %<= 5.0 %ASTM D702
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.491.49ASTM D542
Haze 2.0 %2.0 %ASTM D1003
Transmission, Visible 92 %92 %ASTM D1003
 
Descriptive Properties
FlammabilityB2
Smoke Developed Index550ASTM E84

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Acrylic, Optical Sheet
Röhm Plexiglas® XT Grey 99561 RP Extruded Acrylic Sheet
Corning 9754 Clear Germanate IR Transmitting Glass
Chi Mei Acryrex® CM-205 PMMA
Plaskolite Optix® Acrylic Sheet

PPLAS910 / 150438

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.