MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Samyang Tribit® 1500GN15 Polybutylene Terephthalate, 15% Glass Reinforced, Flame Retardant
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant

Material Notes: Characteristics:
  • G/F reinforced
  • Flame retardant
  • Heat and Impact resistant

Applications:

  • Automotive
    • Connector
    • Gear
    • Outdoor handle
    • Ignition system
  • Electronic
    • Connector
    • Gas valve
    • Coil bobbin
    • Switch case
    • Relay case
  • O/A parts

All information provided by Samyang

Key Words: PBT
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.57 g/ccASTM D792
Water Absorption 0.080 %
@Time 86400 sec
ASTM D570
Linear Mold Shrinkage 0.0020 - 0.012 cm/cm
@Thickness 3.00 mm
ASTM D955
Melt Flow 75 g/10 min
@Load 5.00 kg,
Temperature 250 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 120ASTM D785
Tensile Strength, Yield 900 kg(f)/cm²ASTM D638
Elongation at Break 5.0 %ASTM D638
Flexural Yield Strength 1350 kg(f)/cm²ASTM D790
Flexural Modulus 62000 kg(f)/cm²ASTM D790
Izod Impact, Unnotched 5.00 kg-cm/cm
@Thickness 3.17 mm
ASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+16 ohm-cmASTM D257
Dielectric Constant 3.1
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 20.0 kV/mmASTM D149
Dissipation Factor 0.020
@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 120 secASTM D495
 
Thermal PropertiesOriginal ValueComments
CTE, linear 30.0 µm/m-°CASTM D696
Melting Point 226 °C
Deflection Temperature at 0.46 MPa (66 psi) 220 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 205 °CASTM D648
Flammability, UL94 V-0
@Thickness 1.59 mm
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 240 - 260 °C
Middle Barrel Temperature 230 - 250 °C
Front Barrel Temperature 220 - 230 °C
Nozzle Temperature 250 - 270 °C
Melt Temperature 265 °C
Drying Temperature 110 - 130 °C
Dry Time 4 - 6 hour
Moisture Content 0.010 - 0.015 %
Screw Speed 60 - 80 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Samyang Trirex® 3025G10 Polycarbonate, 10% Glass Reinforced
Trinseo EMERGE™ PC 8701-15 Polycarbonate Resin
Samyang Trirex® 3500G20 Polycarbonate, 20% Glass Reinforced
RTP Company RTP 2200 AR 35  Polyetheretherketone (PEEK) Aramid Fiber 35%
RTP Company RTP 2100 AR 5  Polyetherimide (PEI) Aramid Fiber 5%

PSAMY047 / 88129

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.