MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Nylene® PX3422 Nylon 6, Impact Extrusion Grade
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Impact Grade

Material Notes: Dry as molded. Film Grade. Nylene PX3422 is a heat stabilized, high impact modified nylon resin designed for maximum toughness with minimum sacrifice in tensile strength and melting point. PX3422 offers outstanding elongation and good retention of that elongation after 5 days of heat aging at 177 ºC (95% elongation). Optimum processing conditions should provide a melt temperature of 490 - 530ºF at the die.

ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.

Key Words: Polyamide 6
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.08 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 45.0 MPaASTM D638
Elongation at Break 310 %ASTM D638
Flexural Modulus 1.40 GPaASTM D790
Izod Impact, Notched 8.30 J/cmASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 42.0 °CASTM D495
 
Processing PropertiesOriginal ValueComments
Processing Temperature 265 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultramid® 8254 HS BK-102 PA6 (Dry)
Nylene® 733 Nylon 6
Eurotec® Tecomid® NB50 NL IT PA6, impact modified, super tough, natural, extrusion grade
Eurotec® Tecomid® NB50 NL IT PA 6 super tough
E-Polymers TEKAMID® TB120ST Super Tough PA6, DAM

PN6C46 / 54204

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.