MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

CHT ALPATEC 7610/60 C 2 HV RTV Silicone Adhesive Sealant
Categories: Polymer; Thermoset; Silicone; Silicone, RTV, Adhesive/Sealant Grade

Material Notes: Description: This is a 1-part, RTV (Room Temperature Vulcanizing) silicone adhesive sealant. It is one in a range of Acetoxy cure products which are solvent free. During cure, it liberates a very small amount of acetic acid, giving rise to the familiar ‘vinegar’ odour, which quickly dissipates after cure. It exhibits good primer-less adhesion to many substrates including but not limited to; aluminium, nonferrous metals, steel, glass, enamelled surfaces, fabrics ceramics, thermosetting, thermoplastics and wood and cures rapidly at room temperature when in contact with atmospheric moisture. This product is not to be recommended for use with galvanized metals, ferrous metals, copper and its associated alloys or in electronic assemblies.

Key Features

  • Good resistance to chemicals
  • Very good elongation
  • Good resistance to further tearing
  • High transparency
Key Applications:
  • Complies with Oekotex 100
  • Tin free
  • Solvent free
Application: Coating of stocking laces, narrow fabric and other textiles. ALPATEC 7610/60 C 2 HV is ready to use and can be processed directly from the original container e.g. by means of drum assist pumps without prior mixing. Due to the tin-free blocked catalyst, the silicone paste requires temperatures between 70 and 80 °C for 30 to 40 minutes and 5 – 7 % air humidity for a totally nonsticky fixation. Higher air humidity leads to a destruction of the catalyst and higher temperatures lead to a premature skin formation which inhibits the reaction and the silicone layer remains sticky. Special remark: Direct contact of certain cosmetic articles (skin creams) with the silicone layer can lead to a change in colour. We therefore suggest to carry out pre-trials in production and to point this out on the ready-for-use products if necessary.

Cured Product: Measured under standard climate DIN 50 014-23/50-2. Vulcanised material measured after 14 days.

Information provided by CHT Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.02 g/cc0.0368 lb/in³Cured; DIN 53 479, 23
Storage Temperature 5.00 - 30.0 °C41.0 - 86.0 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 2222DIN 53 505
Tensile Strength 1.70 MPa247 psiDIN 53 504, S 3 A
Elongation at Break 400 %400 %DIN 53 504, S 3 A
Tear Strength 1.75 kN/m10.0 pliASTM D 624, Die B
 
Processing PropertiesMetricEnglishComments
Cure Time 8.00 min0.133 hourSkin formation time, paper method; DIN 50 014 - 23/50-2
 30.0 - 40.0 min
@Temperature 70.0 - 80.0 °C
0.500 - 0.667 hour
@Temperature 158 - 176 °F
5 - 7% RH
 
Descriptive Properties
ColorTransparent
Cure typeAcetate
Flow80 mm10 ml

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHTSIL189 / 314672

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.