MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Universal Wire Works No. 1 Cobalt Alloy Welding Wire
Categories: Metal; Nonferrous Metal; Cobalt Alloy; Superalloy

Material Notes: Universal No. 1 is a cobalt-chromium-tungsten alloy suited for applications requiring extreme abrasion resistance at elevated temperatures. Excellent for resistance to corrosion and oxidation where impact resistance is not mandatory. Hardness characteristics remain intact under operating temperatures of 1800°F. The excellent resistance to wear, softening, corrosion and erosion suits Universal No. 1 to severe applications where a hardness of Rc 53 - 59 is required.

Machinability: Carbide tools or grinding.

Information provided by Universal Wire Works for their line of welding wire and filler metal.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.316 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 53 - 59
Tensile Strength, Ultimate 70000 psi
 
Thermal PropertiesOriginal ValueComments
Melting Point 2250 °F
Maximum Service Temperature, Air 1800 °F
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 2.5 %
Chromium, Cr 29.5 %
Cobalt, Co 49.5 - 50.5 %As Remainder
Iron, Fe 2.0 %
Molybdenum, Mo <= 1.0 %
Nickel, Ni 2.0 %
Silicon, Si 1.0 %
Tungsten, W 12.5 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

NUWW354 / 19763

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.