MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
NuSil MED-4755 Ultra High Performance High Consistency Elastomers - Unrestricted Medical Use
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: Description: High consistency rubber, or HCR, consists of high molecular weight polymer combined with silica to produce a material that can be molded, extruded, or calendared into a useful end product. An HCR has the consistency of clay and is primarily formulated in a one or two part system (peroxide and platinum catalysts, respectively).

Important Properties of Adhesives: Most platinum cure high consistency rubbers are two component systems with an easy-to-work-with 1:1 mix ratio. Features of platinum cure high consistency rubbers include the following:

  • Two part (typically)
  • Heat accelerated
  • No byproducts
  • Post cure optional
  • Low percent shrinkage
Comments: Ultra High Tear

Cure System: Platinum

Information provided by NuSil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.15 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 55Typical
 52 - 60Certified
Tensile Strength at Break 7.60 MPaCertified
 11.0 MPaTypical
Tensile Stress at Strain 385 psi
@Strain 100 %
Elongation at Break 500 %Certified
 900 %Typical
Tear Strength 250 pliCertified
 300 pliTypical
 
Processing PropertiesOriginal ValueComments
Cure Time 4.00 hour
@Temperature 177 °C
Post
 10.0 min
@Temperature 138 °C
Working Life 2.00 hour
@Temperature 25.0 °C
 
Descriptive Properties
Plasticity70 mils

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
NuSil MED-4770 Ultra High Performance High Consistency Elastomers - Unrestricted Medical Use
NuSil MED-4055 Silicone Ultra High Performance High Consistency Elastomer - Restricted Medical Use
NuSil MED-4830 Liquid Silicone Rubber - Unrestricted Medical Use
NuSil MED-4805 Liquid Silicone Rubber - Unrestricted Medical Use
NuSil MED-4880 Liquid Silicone Rubber - Unrestricted Medical Use

PNUSIL315 / 142039

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.