MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik TEGOPREN® 5885 Additive
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Product description: TEGOPREN® 5885 is a hydrophobic, non-ionic, polyether siloxane based wetting and dispersing agent.

Application: TEGOPREN® 5885 is a highly efficient substrate wetting additive for a variety of systems:

  • water-based systems as used for paper laminates and other application
  • solvent-based or solvent–containing systems
TEGOPREN® 5885 is a highly efficient dispersing agent, which improves the incorporation of fillers in different types of plastics like EVA, X-PE, PE etc. and therefore suitable for cable compounds. TEGOPREN® 5885 is a highly efficient additive for pulp and paper antifoams based on organic oils or siloxanes to improve their performance.

Benefits: Especially suitable for water-based formulations, where the following advantages can be observed:

  • No or very low foam formation, even if no additional defoamer is used
  • Improves the wetting of low energy substrates due to extreme lowering of the surface tension of water-based systems
  • Improved durability
TEGOPREN® 5885 is a hydrophobic surfactant with a high affinity to fillers. The use in the production of cable compounds shows outstanding advantages like:
  • improved dispersing of fillers
  • better hydrophobicity
  • smooth and supple cable surfaces
  • no influence on afterwards printing
By use of TEGOPREN® 5885 in pulp and paper defoamer formulations, the following benefits can be achieved:
  • Improved knock down and hold down of defoamers containing TEGOPREN® 5885
  • Better high pH stability versus conventional polyethersiloxane boosted defoamers
  • Cost savings based on better fiber wetting during brown stock washing and bleaching

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.00 g/cc
Viscosity 100 cP
 
Optical PropertiesOriginal ValueComments
Gardner Color Number <= 10
 
Descriptive Properties
Appearanceclear to slightly turbid, yellowish to brownish
Content100%Active matter

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik TEGOPREN® 5852 Additive
Evonik TEGO® Antifoam 2290 Antifoam concentrate
Evonik TEGOPREN® 5847 Additive
Evonik TEGOPREN® 5863 Defoamer
Evonik TEGOPREN® 5851 Defoamer

PEVONIL603 / 196807

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.