MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Mocom (ALBIS) ALCOM® PWL 10/1.1AS UV WT1127-11LB PC, UV stabilized
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: Base Polymer: Polycarbonate

Filler/Additive System: 15% Special filler, antistatic - short term, UV stabilized

Special Features: Highly reflective, opaque

Market Segment: Automotive, various

Application Area: Lighting, light blocking components

Typical Applications: Light guides, reflectors

Information provided by Albis Plastics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.36 g/ccISO 1183
Linear Mold Shrinkage 0.0030 - 0.0060 cm/cm
@Time 86400 sec
ISO 294-4
Melt Flow 22 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 123 MPaH358/30; ISO 2039-1
Tensile Strength 62.0 MPaISO 527
Elongation at Break 50 %ISO 527
Tensile Modulus 2690 MPaISO 527
Flexural Strength 95.0 MPaISO 178
Flexural Modulus 2780 MPaISO 178
Charpy Impact Unnotched NBISO 179/1eU
Charpy Impact, Notched 20.0 kJ/m²ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 138 °CB50; ISO 306
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 89 %Y10 of Reflection; DIN 5033
 0.30 %
@Thickness 0.500 mm
Y10 of Transm.; ISO 13468
 
Processing PropertiesOriginal ValueComments
Melt Temperature 280 - 320 °CInjection molding
Mold Temperature 80.0 - 100 °CInjection molding
Drying Temperature 100 - 120 °C
@Time 14400 - 43200 sec
in air circulating dryer
 120 °C
@Time 7200 - 10800 sec
in a dry air (desiccant) dryer
 
Descriptive Properties
Base PolymerPolycarbonate

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PALBIS8201 / 242260

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.