MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Erbslöh Aluminium DISPAL S541 Aluminum Alloy, AlMg6Mn4SiTiZr, Condition F
Categories: Metal; Nonferrous Metal; Aluminum Alloy

Material Notes:

Information provided by PEAK Werkstoff GmbH, a part of Erbslöh Aluminium GmbH.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.584 - 2.856 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers >= 130HV30
Tensile Strength at Break >= 95.0 MPa
@Temperature 300 °C
 >= 161 MPa
@Temperature 250 °C
 >= 225 MPa
@Temperature 200 °C
 >= 313 MPa
@Temperature 150 °C
 >= 411 MPa
@Temperature 100 °C
 >= 435 MPa
@Temperature 20.0 °C
Tensile Strength, Yield >= 56.0 MPa
@Temperature 300 °C
 >= 114 MPa
@Temperature 250 °C
 >= 182 MPa
@Temperature 200 °C
 >= 251 MPa
@Temperature 150 °C
 >= 286 MPa
@Temperature 100 °C
 >= 305 MPa
@Temperature 20.0 °C
Elongation at Break >= 5.7 %
@Temperature 20.0 °C
 >= 8.4 %
@Temperature 100 °C
 >= 31.2 %
@Temperature 150 °C
 >= 39.4 %
@Temperature 200 °C
 >= 45 %
@Temperature 250 °C
 >= 50 %
@Temperature 300 °C
Modulus of Elasticity >= 41.0 GPa
@Temperature 300 °C
 >= 55.0 GPa
@Temperature 250 °C
 >= 58.0 GPa
@Temperature 200 °C
 >= 64.0 GPa
@Temperature 150 °C
 >= 70.0 GPa
@Temperature 100 °C
 >= 77.0 GPa
@Temperature 20.0 °C
Poissons Ratio 0.324
@Temperature 20.0 °C
 0.33
@Temperature 100 °C
 0.331
@Temperature 150 °C
 0.333
@Temperature 200 °C
 0.336
@Temperature 300 °C
Fatigue Strength 225.8 MPaP50% rotary bending values for 5X107 cycles
 225.8 MPa
@# of Cycles 5.00e+7
P50% rotary bending value
Shear Modulus 24.0 GPa
@Temperature 300 °C
 27.0 GPa
@Temperature 200 °C
 28.0 GPa
@Temperature 150 °C
 29.0 GPa
@Temperature 100 °C
 31.0 GPa
@Temperature 20.0 °C
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000880 - 0.00000970 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 21.8 - 22.8 µm/m-°C
@Temperature 20.0 - 100 °C
 22.6 - 23.6 µm/m-°C
@Temperature 20.0 - 200 °C
 23.4 - 24.4 µm/m-°C
@Temperature 20.0 - 300 °C
Melting Point 570 - 792 °C
Solidus 570.3 - 576.3 °C
Liquidus 785.8 - 791.8 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 87 %As Balance
Magnesium, Mg 6.0 %
Manganese, Mn 4.0 %
Silicon, Si 1.0 %
Titanium, Ti 1.0 %
Zirconium, Zr 1.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Erbslöh Aluminium DISPAL S220 Aluminum Alloy, AlSi35, Condition O
Erbslöh Aluminium DISPAL S225 Aluminum Alloy, AlSi35Fe2Ni, Condition F
Erbslöh Aluminium DISPAL S542 Aluminum Alloy, AlMg6Mn4SiTiZrCo, Condition F
Aluminum 514.0-F, Sand Cast
Erbslöh Aluminium DISPAL S256 Aluminum Alloy, Condition F

NPEAK06c / 143032

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.