MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lubrizol Pearlbond™ 920 Thermoplastic Polyurethane
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Type: Polycaprolactone copolyester-based Aliphatic Thermoplastic Polyurethane with 82 Shore A Hardness.

Features: Translucent resin with excellent color stability upon UV exposure.

Uses: Hotmelt adhesives

Applications: Pearlbond™ 920 is suitable for use in blown extrusion, slot-die extrusion, roll coating and powder applications where the following features are of high value to the customer: Fast crystallization rate; Low activation temperature; Excellent bonding strength; High resistance to UV

Information provided by The 159 Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.11 g/ccISO 2781 / ASTM D-792
Melt Flow 15 - 35 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 82
@Time 3.00 sec
ISO 868 / ASTM D-2240
Tensile Strength 38.4 MPaISO 527
Tensile Stress at Strain 5.40 MPa
@Strain 100 %
ISO 527
 10.5 MPa
@Strain 300 %
ISO 527
Elongation, Ultimate 723 %ISO 527
Tear Strength 80.0 kN/mISO 34-1B (ASTM D-624 Die C)ISO 34-1B (ASTM D-624
 
Thermal PropertiesOriginal ValueComments
Melting Point 110 - 135 °CMQSA 70A
Vicat Softening Point 60.0 °CA50; ISO 306
 
Processing PropertiesOriginal ValueComments
Zone 1 175 - 185 °C
Zone 2 180 - 190 °C
Zone 3 180 - 190 °C
Zone 4 175 - 185 °C
Die Temperature 165 - 175 °C
Dry Time 3.00 hour
@Temperature 70.0 °C
 
Descriptive Properties
Activation temperature110-120°CLA-17

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLUBR5043a / 278125

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.