Solid content(%): 16±1%
Film forming resin: Cellulose ether
Viscosity (4# rotor, 30 rpm, 25 centigrade): <15Pa.s
Volume resistivity: 0.06-0.08O·cm, at 10µm
Curing condition: 20-25min at 150 centigrade
Instructions: Stir well before use to restore fluidity. 150-200 mesh screen printing on substrates such as paper, PET film. Can be washed directly with alcohol or butyl acetate. |