MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Morgan Advanced Ceramics Kaowool® Paper 500 Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: RCF fiber class. High-performance paper and felt products from Thermal Ceramics are the preferred choice over traditional fiberglass, textile, or metal products for thermal, acoustical, or filtration management. Kaowool Flex-Wrap is produced from a blend of Kaowool high purity ceramic fibers and organic binders. Due to its low organic binder content, offgassing is at a minimum. This specialty paper is noted for its excellent flexibility, outstanding handling characteristics, and high insulating value at high temperatures. Kaowool 500, 700, and 900 Grade paper products are produced from Kaowool high purity fibers and organic binders. Each of these paper products are noted for their excellent tensile strengths and outstanding handling characteristics.

Applications:

  • High temperature gaskets and seals
  • Refractory back-up insulation
  • Appliance insulation
  • Separating media for heat treating metals
  • High temperature filtration
  • High temperature expansion joint packing
  • Glassware separating media
  • Parting agent for brazing operations
  • Hot face and backup lining for lab furnaces
  • Aluminum distributor pan lining
  • Super alloy ingot mold lining and hot tapes

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.192 - 0.224 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 0.0100 - 0.0200 MPafired
 0.510 - 0.680 MPa
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.0600 W/m-K
@Temperature 260 °C
ASTM C201
 0.0900 W/m-K
@Temperature 538 °C
ASTM C201
 0.150 W/m-K
@Temperature 816 °C
ASTM C201
 0.230 W/m-K
@Temperature 1093 °C
ASTM C201
Melting Point 1760 °C
Maximum Service Temperature, Air 1176 °CContinuous Use
 
Component Elements PropertiesOriginal ValueComments
Al2O3 47 %
Loss on Ignition(%) 6.0 - 10 %
SiO2 53 %
 
Descriptive Properties
Classification Temperature (°C)1260
Colorwhite
Fiber Index0.5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ThyssenKrupp PAS 700 Structural Steel for Cold Forming
Chosun Refractories HSC-18RA Dense and High-Strength Castable, Superdense
Chosun Refractories HSC-15 Dense and High-Strength Castable, Credens

CMORF7074 / 203373

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.