MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Ascend Performance Materials Vydyne® 840C Nylon 66, Extrusion Grade  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Extruded; Nylon 66, Film

Material Notes: 840C is a PA66-based copolymer that features high melt strength, shear thinning behavior, high tensile strength, ductility, and high clarity making it ideal for blown or cast film applications. Specifically, its combination of high temperature resistance, good clarity, and toughness makes it a very useful and versatile material in a number of multi-layer, flexible packaging applications.

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.674 g/ccASTM D1895
Density 1.14 g/ccISO 1183
Moisture Absorption 0.100 %ASTM D6869
Viscosity Measurement 3.9 - 4.1Relative Viscosity - Sulfuric Acid; ISO 307
 110 - 140Relative Viscosity - Formic Acid; ASTM D789
 
Thermal PropertiesOriginal ValueComments
Melting Point 235 °CISO 11357-3
 
Processing PropertiesOriginal ValueComments
Processing Temperature 20.0 - 40.0 °CBlow Film Air Temperature
 245 - 265 °CCylinder - Extrusion
Die Temperature 255 - 275 °CExtrusion
 70.0 - 80.0 °C
@Time 0.000 - 14400 sec
Extrusion
Melt Temperature 235 °CExtrusion
Moisture Content 0.030 - 0.080 %Extrusion
 
Compliance PropertiesOriginal ValueComments
European Food 1935/2004 Yes
 
Descriptive Properties
Agency RatingsAgency Ratings
 EU 10/2011
 EU 2023/2006
FeaturesChemical Resistant
 Good melt strength
 High Melt Stability
 High Strength
 High Toughness
 Puncture resistant
Melt Pressure MPa3-17
Screw DesignGP or Barrier
UsesIndustrial Applications
 Monofilaments
 Multilayer film
 Profiles
 Rods
 Sheet
 Tubing
 Vacuum Bagging Film

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PZASCE9773 / 220876

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.