MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Graft Polymer GRAFTABOND™ PO-SAN 00647 IM Polyethylene Octene, grafted with Styrene Acrylonitrile
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: GRAFTABOND™ PO-SAN 00647 IM is Polyethylene octene grafted with SAN. This product provides enhanced impact strength to the base material, while also maintaining compatibility with polymers that contain nitrile and amide groups.

Applications:

  • GRAFTABOND™ PO-SAN 00647 IM is a great additive for increasing impact strength of soft materials
  • Excellent compatibility with polymers, containing nitrile or amide groups (e.g. SAN, ABS).
Supplied as: Powder.

Properties can be regulated to customer needs.

Information provided by Graft Polymer LTD.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Chemical PropertiesOriginal ValueComments
Styrene Content 4.0 %By FTIR
 
Descriptive Properties
Acrylonitrile Content4%FTIR
Drying Loss<0.5 g/cc. ASTM D6980.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Graft Polymer GRAFTABOND™ PPC-GMA 02030 C Polypropylene grafted with Glycidyl Methacrylate
Graft Polymer GRAFTABOND™ SB-GMA 00330 C Styrene Butadiene Copolymer Grafted with Glycidyl Methacrylate
Graft Polymer GRAFTABOND™ PPH-MAH 02030 C Maleic anhydride functioned homo-polypropylene
Graft Polymer GRAFTABOND™ PO-MAH 00410 IM Polyethylene Octene grafted with Maleic Anhydride
Graft Polymer GRAFTABOND™ PO-GMA 00617 Polyethylene Octene grafted with glycidyl methacrylate

PGRAFT938 / 232369

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.