MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
JIS S55C Steel, Normalized
Categories: Metal; Ferrous Metal; Carbon Steel; AISI 1000 Series Steel; Medium Carbon Steel

Material Notes: Very common grade in Asia.

Key Words: Similar to AISI 1050 and 1055 and DIN CK55.
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.85 g/ccAISI 1055
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 183 - 255
Hardness, Rockwell C 9.0 - 24.5
Tensile Strength, Ultimate 6600 kg(f)/cm²
Tensile Strength, Yield 4000 kg(f)/cm²
Elongation at Break 15 %
Modulus of Elasticity 205 GPaTypical steel
Poissons Ratio 0.29Typical steel
Machinability 55 %Based on AISI 1212 steel as 100% machinability
Shear Modulus 80.0 GPaTypical steel
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000163 ohm-cm
@Temperature 0.000 °C
condition of specimen unknown
 
Thermal PropertiesOriginal ValueComments
CTE, linear 11.0 µm/m-°C
@Temperature 20.0 - 100 °C
 12.4 µm/m-°C
@Temperature 0.000 - 300 °C
 13.9 µm/m-°C
@Temperature 0.000 - 500 °C
Specific Heat Capacity 0.486 J/g-°C
@Temperature 50.0 - 100 °C
(AISI 1045) annealed
Thermal Conductivity 49.8 W/m-KTypical steel
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.52 - 0.58 %
Chromium, Cr <= 0.20 %
Copper, Cu <= 0.30 %
Iron, Fe 97.5 - 98.7 %
Manganese, Mn 0.60 - 0.90 %
Nickel, Ni <= 0.20 %
Phosphorus, P <= 0.030 %
Silicon, Si 0.15 - 0.35 %
Sulfur, S <= 0.035 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
JIS S55C Steel, Tempered
Bohler-Uddeholm SUPERIOR® H13 Hot Work Tool Steel
Assab Steels 760 Machinery Steel
JIS S45C Steel, Normalized
JIS S45C Steel, Tempered

MSJ55Ca / 14083

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.