MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Top Polymer Topolymer® 8219-P TPE
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Production Description: Topolymer® 8219-P is an easy processing compound , which made from Kraton & Kuraray polymer. 8219-P overmolded designs are valuable in applications for polymer bonding such as PC, ABS, PC/ABS and SAN etc. by injection

Features: Excellent tear resistant, flexibility, weatherability and heat resistant Excellent bonding ability with PC, ABS, PC+ABS and SAN etc.

Information provided by Top Polymer Enterprise

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.920 - 1.05 g/cc
Linear Mold Shrinkage 0.015 - 0.020 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 50 - 99
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 120 - 160 °CInjection
Middle Barrel Temperature 180 - 220 °CInjection
Front Barrel Temperature 180 - 220 °CInjection
Nozzle Temperature 160 - 180 °CInjection
Mold Temperature 40.0 - 60.0 °CInjection
Injection Pressure 3.00 - 10.0 MPaInjection
Screw Speed 30 - 80 rpmInjection
 
Descriptive Properties
ColorNatural, foggy
Screw L/D22:1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Elix Polymers ELIX™ 190 TE Acrylonitrile Butadiene Styrene (ABS), PTFE Reinforced
Top Polymer Topolymer® 8200-T/C/A TPE
Top Polymer Topolymer® 8229-P TPE
Top Polymer Topolymer® 8209-P TPE
SEKISUI SPI ALLEN® Alextra™ MV PC/PC+ABS

PTOPO046 / 184558

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.