MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Corning Vycor® 7950 Red Glass  (discontinued **)
Categories: Ceramic; Glass; Optical; Oxide; Silicon Oxide

Material Notes: Used to reduce the light of quartz lamps (blocks most visible white light while transmitting IR). One specific use is blocking glare from heating units.

Special Features:

  • Superior optical quality
  • Tight dimensional control
  • Thermal and chemical properties ideally suited to high temperatures.
  • Excellent thermal shock resistance

Information provided by Corning Incorporated.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.18 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Knoop 487KHN100
Modulus of Elasticity 66.2 GPa
Poissons Ratio 0.19
Shear Modulus 28.0 GPa
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.30e+8 ohm-cm
@Temperature 350 °C
 5.00e+9 ohm-cm
@Temperature 250 °C
Dielectric Constant 3.8
@Frequency 1e+6 Hz
Dissipation Factor 0.00040
@Frequency 1e+6 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 0.750 µm/m-°C
@Temperature 0.000 - 300 °C
Specific Heat Capacity 0.750 J/g-°C
Thermal Conductivity 0.00330 cal cm/sec-cm²-°C
Maximum Service Temperature, Air 900 °CContinuous
Softening Point 1530 °C107.6 Poise
Annealing Point 1020 °C1013 Poise
Strain Point 890 °C1014 Poise
 
Optical PropertiesOriginal ValueComments
IR Transmittance 60 %
@Wavelength 800 nm
 65 %
@Wavelength 1500 nm
 
Component Elements PropertiesOriginal ValueComments
SiO2 96 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Goodfellow Vycor® 7913 Glass
Corning Macor® Machinable Glass Ceramic
Corning Pyroceram® Code 9606 Glass Ceramic
Corning Vycor® 7907 UV-Blocking Glass
Corning Vycor® 7930 Porous Glass

CCORNV05 / 751

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.