Description: Nilamid A3 H ZE was developed for applications which are subjected to very high shock loads, also at minus temperatures. It has good impact performance, whilst maintaining good strength and stiffness. It is an easy to mould material, that can be supplied with a full spectrum of colors. Key characteristics: - Good impact performance, also at minus temperatures
- Good thermal performance
- Good strength and stiffness
- Easy processing
- Available in a wide range of colors
Information provided by NILIT. |