MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lucite International Colacryl® TS1875 Acrylic Solution Resin
Categories: Polymer; Thermoplastic; Acrylic (PMMA)

Material Notes: Colacryl TS 1875 is a self cross-linking acrylic copolymer designed for high performance solvent resistant adhesive applications. Once dried, a film cast from this product remains permanently tacky.

Suggested Uses: Pressure-sensitive self-adhesive products including high shear double-sided tapes and films which require a high degree of solvent resistance.

Polyacrylate copolymer

Information provided by Lucite International

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 49 - 53 %49 - 53 %
Viscosity 1500 - 7500 cP
@Temperature 25.0 °C
1500 - 7500 cP
@Temperature 77.0 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 6.00 Month6.00 Month
 
Descriptive Properties
SolventAcetone N

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lucite International Colacryl® D120 Acrylic Dental Resin
Lucite International Colacryl® D60 Acrylic Dental Resin
Lucite International Colacryl® D150 Acrylic Dental Resin
Lucite International Colacryl® TS2050 Acrylic Resin
Lucite International Colacryl® D80FC Acrylic Dental Resin

PLUCIT9442 / 150156

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.