MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
RTP Company RTP 1200 S-55D Ester-based Thermoplastic Polyurethane Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane TPE; Polyurethane, TP

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.22 g/ccASTM D 792
Linear Mold Shrinkage 0.0090 cm/cm
@Thickness 3.20 mm
ASTM D 955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 58instantaneous; ASTM D 2240
Tensile Strength at Break 6034 psiASTM D 412
Tensile Stress at Strain 2220 psi
@Strain 50 %
ASTM D 412
 2350 psi
@Strain 100 %
ASTM D 412
 5200 psi
@Strain 300 %
ASTM D 412
Elongation at Break 561 %ASTM D 412
Flexural Modulus 25000 psiASTM D 790
Tear Strength 990 pliDie C; ASTM D 624
Compression Set 25 %
@Temperature 23.0 °C,
Time 79200 sec
Method B; Type 2; ASTM D 395
 
Processing PropertiesOriginal ValueComments
Melt Temperature 400 - 430 °F
Mold Temperature 80.0 - 140 °F
Drying Temperature 225 °F
@Time 21600 sec
Moisture Content 0.020 %
Dew Point -20.0 °F
Injection Pressure 6000 - 15000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
RTP Company RTP 1200 S-65D Ester-based Thermoplastic Polyurethane Elastomer
RTP Company RTP 1200 S-40D Ester-based Thermoplastic Polyurethane Elastomer
Huntsman IROGRAN® D 60 E 4024 Polyester-Based TPU-High Performance Grade
Taiwan Sheen Soon Sheenthane® D6010 Thermoplastic Polyurethane Elastomer
Huntsman IROGRAN® A 95 P 5044 DP TPU-Polyether

PQZWA3533 / 91716

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.