MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Petrothene YR92866 LLDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes: Petrothene YR92866 is a low density polyethylene/ethylene vinyl acetate copolymer compound selected for use in wire and cable jacketing applications where extra flexibility is required. The carbon black content of YR92866 is 2.5 percent. Antioxidant has been added to ensure thermal stability during processing. Applications: Wire & Cable

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.940 g/cc0.0340 lb/in³
ESCR 100% Igepal® >= 168 hour>= 168 hour0 failures @ 7 days, cond. A
Carbon Black Loading 2.5 %2.5 %
Melt Flow 0.48 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.48 g/10 min
@Load 4.76 lb,
Temperature 374 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 19.3 MPa2800 psi
Elongation at Break 730 %730 %
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 2.66
@Frequency 1e+6 Hz
2.66
@Frequency 1e+6 Hz
Dissipation Factor 0.0090
@Frequency 1e+6 Hz
0.0090
@Frequency 1e+6 Hz
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature <= -76.0 °C<= -105 °F
 
Descriptive Properties
Processing MethodWire & Cable

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Braskem HF3712 Extrusion Linear Low Density Polyethylene
NOVA Chemicals Novapol® TF-Y534-IP Hexene LLDPE Film Resin
ExxonMobil LLDPE LL 3402.48 Blown Linear Low Density Polyethylene Resin
ExxonMobil Exceed™ 3505MC Film Grade Hexene LLDPE
Dow DOWLEX™ 2553 Linear Low Density Polyethylene, Narrow MW Distribution

PEQT8885 / 220519

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.