MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

LyondellBasell Hifax™ CB229 Thermoplastic Olefin Resin  (discontinued **)
Categories: Polymer; Thermoplastic

Material Notes:
Key Features: medium high melt flow, medium high modulus, paintable thermoplastic elastomeric olefin resin, excellent impact and stiffness balance, good dimensional stability, excellent processability, good paintability

Applications: automotive claddings and rocker panels, end caps, appliques

Description: Hifax CB229 medium melt flow, mineral-filled thermoplastic elastomeric olefin resin has an excelent combination of flow, stiffness, paintability and dynamic impact characteristics. It was designed primarily for automotive exterior ornamentation applications.

Information provided by Montell Polyolefins.

LyondellBasell is the successor company to Montell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.990 g/cc0.0358 lb/in³ISO 1183
Linear Mold Shrinkage 0.010 cm/cm0.010 in/inTool, Montell
Melt Flow 11 g/10 min
@Load 2.16 kg,
Temperature 230 °C
11 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6565ISO 868
Tensile Strength, Ultimate 17.0 MPa2470 psiISO R527-1
Tensile Strength, Yield 20.0 MPa2900 psiISO R527-1
Elongation at Break >= 500 %>= 500 %ISO R527-1
Elongation at Yield 10 %10 %ISO R527-1
Flexural Modulus 1.30 GPa189 ksiISO 178
Izod Impact, Notched 0.350 J/cm0.656 ft-lb/inISO 180
Impact Test 24.0 J
@Temperature -30.0 °C
17.7 ft-lb
@Temperature -22.0 °F
MAII, E at Max Load, Ductile; ISO 6603-2
 
Thermal PropertiesMetricEnglishComments
CTE, linear 66.0 µm/m-°C
@Temperature -30.0 - 100 °C
36.7 µin/in-°F
@Temperature -22.0 - 212 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 85.0 °C185 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C122 °FISO 75

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Hifax™ CJ232 Thermoplastic Olefin Resin
Noble Polymers Ecobarrier™ 0916 Thermoplastic Olefin (TPO)
LyondellBasell Hifax™ TRA-3263EC/1 Thermoplastic Olefin Resin
LyondellBasell Hifax™ ETA-3163 Thermoplastic Olefin Resin
LyondellBasell Hifax™ CB228 Thermoplastic Olefin Resin

PMO456 / 53641

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.