MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Phillips 66 Triton® Grade 460
Categories: Fluid; Lubricant; Lithium Gellant; Polyalphaolefin (PAO)

Material Notes: Phillips 66® Triton is a premium quality, synthetic, extreme-pressure (EP) lithium complex grease specifically developed to provide outstanding protection for industrial and automotive equipment operating at extreme temperatures or over a wide temperature range. It is available in three grades to cover a wide range of applications. Triton is manufactured with synthetic polyalphaolefin (PAO) base oils and a lithium complex soap thickener. It is fortified with extreme-pressure and antiwear additives plus rust and oxidation inhibitors to provide excellent wear protection, protection against rust and corrosion, and long service life. It has outstanding oxidation resistance at high temperatures and outstanding pumpability at low temperatures. Triton 100 is an NLGI No. 2 grease formulated with an ISO VG 100 base oil. It is recommended for lubrication of lightly loaded, high-speed bearings such as those found in electric motors and fans. Triton 220 is an NLGI No. 2 grease formulated with an ISO VG 220 base oil. It is NLGI GC-LB certified for use as an automotive wheel bearing and chassis grease, and also is recommended for lubrication of medium-speed bearings in industrial equipment. Triton 460 is a heavy-duty, NLGI No. 1.5 grease formulated with an ISO VG 460 base oil. It is recommended for lubrication of low- to medium-speed bearings in industrial, mining and mobile equipment operating under heavy loads and/or wet conditions.

Applications:

  • Lightly loaded, high-speed bearings in electric motors and fans (100 grade)
  • Chassis parts and wheel bearings on passenger cars, trucks and other mobile equipment (220 grade)
  • Heavily loaded plain and rolling-element bearings in industrial, mining and marine equipment, and in off-highway mobile equipment (220 & 460 grades)
Features/Benefits:
  • Outstanding oxidation resistance and thermal stability at high temperatures
  • Outstanding pumpability at low temperatures
  • Excellent wear protection for longer equipment life
  • High load-carrying capacity
  • Protects against rust and corrosion
  • Good resistance to water washout
  • NLGI GC-LB certified (220 grade)

Information provided by Phillips 66 Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.868 g/cc0.0313 lb/in³
Viscosity Measurement 150150Index
Saybolt Viscosity at 100°F 2400 SUS2400 SUS
Saybolt Viscosity at 210°F 214 SUS214 SUS
Kinematic Viscosity at 40°C (104°F) 460 cSt460 cSt
Kinematic Viscosity at 100°C (212°F) 44.3 cSt44.3 cSt
Oxidative Stability 100 hour
@Pressure 0.0345 MPa
100 hour
@Pressure 5.00 psi
ASTM D942
 
Mechanical PropertiesMetricEnglishComments
Four Ball Extreme Pressure, Weld Load 250 kg551 lb (mass)ASTM D2596
Four Ball Wear 0.600 mm0.0236 inScar Diameter; ASTM D2266
Penetration 295 - 310295 - 31060 strokes; ASTM D217
Timken Test 24900 g55.0 lbASTM D2509
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 177 °C351 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °F
Dropping Point >= 260 °C>= 500 °F
 
Descriptive Properties
ColorPurple
ThickenerLithium Complex
US Steel Mobility1.8 g/min-40°C, LT37
 10.2 g/min-18°C, LT37
 28.8 g/min-7°C, LT37
 3 g/min-29°C, LT37
 66 g/min4°C, LT37
Water Washout Resistance<6%Weight Loss @ 175°F, ASTM D1264

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WCON5447 / 198700

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.