MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik DYNACOLL® Terra EP 424.01 Polyester-Polyol
Categories: Polymer; Renewable/Recycled Polymer; Thermoset; Polyester, TS

Material Notes: Bio-based Polyester-Polyols: With its DYNACOLL® Terra product range Evonik offers polyester-polyols made from renewable raw materials. These bio-based polyesters contain between > 30 and 100 ppw of renewable monomers. According to our DYNACOLL® 7000 product range a building block system of medium molecular weight copolyesters for moisture curing PUR hot melts was developed. It is divided in three basic groups:
  • Amorphous Grades
  • Liquid Grades
  • Crystalline Grades
DYNACOLL® Terra bio-based polyesters are usually supplied in 25 or 30 kg and 190 or 200 kg steel drums.

Your benefits:

  • support of resource efficiency by using green components
  • modular combination of polyesters in RHM formulation possible
  • available grades exhibiting broad range of properties in formulations
  • well-balanced and versatile adhesion properties
  • implementation of new properties possible

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 4.0 cP
@Temperature 80.0 °C
DIN EN ISO 3219
 4.0 cP
@Temperature 130 °C
Reactive Hot Melt; DIN EN ISO 3219
Molecular Weight 3500 g/mol
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 10.0 MPaReactive Hot Melt
Elongation at Break 1300 %
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg -40.0 °CDIN 53765
 
Descriptive Properties
Hydroxyl Number30 mg KOH/gDIN 53 240-02
Proportion of Renewables>85%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik DYNACOLL® Terra EP 413.01 Polyester-Polyol

PEVONIL117 / 196321

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.