MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Matexcel NAT-4005 Hydrophobic Nanocellulose
Categories: Wood and Natural Products

Material Notes: Hydrophobic nanocellulose functional additives are based on nanocellulose materials prepared from corncob cellulose, and are modified by siloxane groups with high chemical reactivity on the silane coupling agent. A hydrophobic three-dimensional structure in the form of a hydrophobic Si-O-C is formed to achieve a superhydrophobic effect like a lotus leaf.

NAT-4005; Hydrophobic Nanocellulose; nanocellulose product

Application: Supermarket paper bags, tote bags, waterproof and moisture-proof packaging, etc.

Morphology: Milky white hydrogel

Key Words: Synonyms: Hydrophobic Nanocellulose
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Storage Temperature 20.0 °C
 
Descriptive Properties
Product overviewFiber diameter: =60nm Aspect ratio: =200 Concentration: 4%-4.5% ph value: 6-7 The hydrophobic angle can be greater than 140°, and the rolling angle is less than 10°

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMXCK2103 / 300734

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.