MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
E-Polymers SEPAZ® C230GI 30% Glass Fiber Reinforced Good Impact LCP Resin
Categories: Polymer; Thermoplastic; Liquid Crystal Polymer (LCP); Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled

Material Notes: Liquid Crystal Polymer Resin: SEPAZ LCP resin has a unique structure and performance unthought of in a traditional plastics. Beside SEPAZ LCP takes the excels in all-around performance and molding productivity. SEPAZ LCP has a unique attribute in that the thinner the product becomes, the greater the mechanical strength. SEPAZ LCP finds uses in connectors, sensors and other electronic components and CD pick-up parts, and in copying machine and fax components in office and audio-visual equipment.

Information Provided by E-Polymers Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.62 g/ccASTM D792
Linear Mold Shrinkage 0.00 cm/cm
Linear Mold Shrinkage, Transverse 0.0090 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 150.1 MPaASTM D638
Elongation at Break 1.7 %ASTM D638
Flexural Strength 183.45 MPaASTM D790
Flexural Modulus 13100 MPaASTM D790
Izod Impact, Notched 22.0 kg-cm/cmASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+13 ohm-cmASTM D257
Surface Resistance 1.00e+15 ohmASTM D257
Dielectric Constant 3.8
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 24.0 kV/mm
@Thickness 1.60 mm
ASTM D149
Dissipation Factor 0.029
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 14.0 µm/m-°C
@Thickness 1.60 mm
ASTM D696
CTE, linear, Transverse to Flow 36.0 µm/m-°C
@Thickness 1.60 mm
ASTM D696
Melting Point 352 °CASTM D789
Deflection Temperature at 1.8 MPa (264 psi) 289 °CASTM D648
Flammability, UL94 V-0
 
Processing PropertiesOriginal ValueComments
Melt Temperature 365 - 375 °C
Mold Temperature 30.0 - 150 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Avient Therma-Tech™ LC-6000 TC Liquid Crystal Polymer (LCP)
Avient Therma-Tech™ LC-5000C TC LCP
Celanese CoolPoly® D5506 Thermally Conductive Liquid Crystalline Polymer
Celanese CoolPoly® D5502 Thermally Conductive Liquid Crystalline Polymer
Celanese VECTRA A530 LCP, 30% Mineral Reinforced

PEPOLZ067 / 103564

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.