MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DuPont Mobility and Materials Rynite® FR530L NC010 Polyethylene Terephthalate (PET)  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant

Material Notes:

Rynite FR530 NC010 is a 30% glass reinforced flame retardant modified polyethylene terephthalate resin.

While this product line has been acquired by Celanese, this specific grade had been disconued while still a DuPont product so it is listed here as a discontinued DuPont product.

Key Words: PET-GF30FR(17)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.68 g/ccISO 1183
Water Absorption 0.75 %
@Thickness 2.00 mm
Sim. to ISO 62
Moisture Absorption 0.150 %
@Thickness 2.00 mm
Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0020 cm/cmISO 294-4 2577
Linear Mold Shrinkage, Transverse 0.0080 cm/cmISO 294-4 2577
Melt Flow 6.0 g/10 min
@Load 2.16 kg,
Temperature 280 °C
cm³/10min; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 95ASTM D785
Hardness, Rockwell R 120ASTM D785
Tensile Strength at Break 135 MPaISO 527-1/-2
Elongation at Break 2.0 %ISO 527-1/-2
Tensile Modulus 11500 MPaISO 527-1/-2
Flexural Modulus 10500 MPaISO 178
Shear Modulus 0.525 GPa
@Temperature 160 °C
Dynamic; ISO 11403-1 -2
 0.654 GPa
@Temperature 120 °C
Dynamic; ISO 11403-1 -2
 1.151 GPa
@Temperature 70.0 °C
Dynamic; ISO 11403-1 -2
 1.974 GPa
@Temperature 20.0 °C
Dynamic; ISO 11403-1 -2
 2.208 GPa
@Temperature -20.0 °C
Dynamic; ISO 11403-1 -2
 2.432 GPa
@Temperature -50.0 °C
Dynamic; ISO 11403-1 -2
Charpy Impact Unnotched 40.0 kJ/m²ISO 179/1eU
 40.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
Charpy Impact, Notched 10.0 kJ/m²ISO 179/1eA
 9.00 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
Tensile Creep Modulus, 1 hour 11200 MPa
@Time 3600 sec
ISO 899-1
Tensile Creep Modulus, 1000 hours 9700 MPa
@Time 3.60e+6 sec
ISO 899-1
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+14 ohmIEC 60093
Dielectric Constant 3.7
@Frequency 1e+6 Hz
ASTM D150
 3.8
@Frequency 1000 Hz
ASTM D150
 4.7
@Frequency 1e+6 Hz
IEC 60250
 4.8
@Frequency 100 Hz
IEC 60250
Dielectric Strength 33.0 kV/mmIEC 60243-1
Dissipation Factor 0.0070
@Frequency 100 Hz
IEC 60250
 0.010
@Frequency 1e+6 Hz
IEC 60250
 0.011
@Frequency 1000 Hz
ASTM D150
 0.018
@Frequency 1e+6 Hz
ASTM D150
Comparative Tracking Index 225 VIEC 60112
 250 - 400 VUL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 19.0 µm/m-°CISO 11359-1/-2
 22.0 µm/m-°C
@Temperature -40.0 - 23.0 °C
ISO 11359-1/-2
CTE, linear, Transverse to Flow 92.0 µm/m-°CISO 11359-1/-2
 68.0 µm/m-°C
@Temperature -40.0 - 23.0 °C
ISO 11359-1/-2
Melting Point 252 °C10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 243 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 225 °CISO 75-1/-2
Vicat Softening Point 220 °C50°C/h 50N; ISO 306
UL RTI, Electrical 155 °C
@Thickness 0.400 mm
UL 746B
Flammability, UL94 V-0
@Thickness 1.50 mm
IEC 60695-11-10
 V-0
@Thickness 0.300 mm
IEC 60695-11-10
 5VA
@Thickness 0.900 mm
IEC 60695-11-20
Oxygen Index 33 %ISO 4589-1/-2
 33 %ASTM D2863
 
Descriptive Properties
AdditivesRelease agent
Delivery formPellets
Part Marking Code>PET-GF30FR<ISO 11469
ProcessingInjection Molding
Regional AvailabilityEurope
 Near East/Africa
Resin IdentificationPET-GF30FR(17)
UL recognitionUL

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont Mobility and Materials Rynite® FR530L BK507 Polyethylene Terephthalate (PET)
Celanese Rynite® 408 NC010 PET
DuPont Mobility and Materials Rynite® GW520CS NC010 Polyethylene Terephthalate (PET)
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced
Celanese Rynite® 530 NC010 PET-GF30

PZDSY5281 / 161108

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.