STYPOL® 040-4985 and 040-4988 are clear, light colored, acrylic modified, chemical resistant NPG isophthalic resins designed specifically for spray granite applications where the user incorporates granite effect fillers. Features and Benefits: - Good sprayability
- Excellent nonsagging properties when filled with granite effect fillers
- High clarity
- Light stabilized
- Good color retention
Information provided by Polynt Composites. |