MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Old Hickory UltraCast Slurry PC-2000 Kentucky Ball Clay  (discontinued **)
Categories: Ceramic; Clay; Ball Clay

Material Notes: Slurry grade shipped at 60% solids content and deflocculated with sodium silicate to maintain stable rheology characteristics. It is suitable for a variety of ceramic casting formulations ranging from standards bench cast to pressure cast and capillary type production systems. High permeability with good strength and plasticity is a key property of this slurry grade clay.

Information provided by Old Hickory Clay Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.585 - 1.60 g/cc
Solids Content 60 - 61 %
Particle Size 0.50 µm29% of particles less than
 1.0 µm41% of particles less than
 2.12 µmMedian particle diameter
 <= 5.0 µm71% of particles less than
pH 3.0 - 5.5
@Temperature 32.2 °C
Soluble Sulfates 300 - 500 ppm
Specific Surface Area 16.5 m²/g
Viscosity 100 - 300 cP
@Temperature 32.2 °C
 
Mechanical PropertiesOriginal ValueComments
Modulus of Rupture 0.625 ksiDry Modulus of Rupture, 50% clay/50% flint
 
Component Elements PropertiesOriginal ValueComments
Al2O3 25.14 %
CaO 0.16 %
Carbon, C 1.1 %
Fe2O3 1.41 %
K2O 1.49 %
Loss on Ignition(%) 9.08 %
MgO 0.48 %
Na2O 0.11 %
SiO2 60.59 %
TiO2 1.62 %
 
Descriptive Properties
CEC/MBI (meg/100 ml)6.8
Deflocculant TypeSodium Silicate (N Brand)
Drop On Curve (cps)30-120at 90°F, Brookfield, 100 rpm, No. 3 Spindle

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Silberline SilBerCote® PC 1291X
Tropical Iroko Wood
Abatron WoodEpox® Wood Replacement Compound
Abatron LiquidWood® Deep Penetrating Wood Consolidant
CRP Technology Windform® XT 2.0 Polyamide-Carbon Fiber Composite

EOHC911 / 161990

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.