MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

BASF 3D Ultrafuse® PC GF30 30% Glass Fiber Reinforced, Fused Fillament, Conditioned
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, 30% Glass Filled

Material Notes: Components: Polycarbonate based filament filled with 30% glass fibers for Fused Filament Fabrication.

Product Description: Ultrafuse® PC GF30 is polycarbonate, reinforced with 30% glass fiber content. The fibers in this material are specially designed for 3D-printing filaments and are compatible with a wide range of FFF 3D-printers. The extreme stiffness makes this material highly suitable for demanding applications. Ultrafuse® PC GF30 delivers superior strength and good temperature resistance. With its resilience to UV light and its flame retardancy and V0 verification it is perfectly suitable for various industrial applications.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.176 g/cc0.04249 lb/in³Printed Part; ISO 1183-1
Melt Flow 30.576 g/10 min
@Load 2.16 kg,
Temperature 300 °C
30.576 g/10 min
@Load 4.76 lb,
Temperature 572 °F
ISO 1133
Storage Temperature 15.0 - 25.0 °C59.0 - 77.0 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 11.2 MPa1620 psiZX: Upright; ISO 527
 36.1 MPa5240 psiXY: Flat; ISO 527
Elongation at Break 1.1 %1.1 %ZX: Upright; ISO 527
 2.4 %2.4 %XY: Flat; ISO 527
Modulus of Elasticity 1.231 GPa178.5 ksiYoung's, ZX: Upright; ISO 527
 2.665 GPa386.5 ksiYoung's, XY: Flat; ISO 527
Flexural Strength 19.0 MPa2760 psiZX: Upright; ISO 178
 63.4 MPa9200 psiXY: Flat; ISO 178
 78.8 MPa11400 psiXZ: On its edge; ISO 178
Flexural Modulus 0.934 GPa135 ksiZX: Upright; ISO 178
 2.69 GPa390 ksiXY: Flat; ISO 178
 3.45 GPa500 ksiXZ: On its edge; ISO 178
Flexural Strain at Break 2.5 %2.5 %ZX: Upright; ISO 178
 2.9 %2.9 %XZ: On its edge; ISO 178
 3.2 %3.2 %XY: Flat; ISO 178
Izod Impact, Notched (ISO) 2.10 kJ/m²0.999 ft-lb/in²ZX: Upright; ISO 180
 5.40 kJ/m²2.57 ft-lb/in²XZ: On its edge; ISO 180
 5.60 kJ/m²2.66 ft-lb/in²XY: Flat; ISO 180
Izod Impact, Unnotched (ISO) 3.40 kJ/m²1.62 ft-lb/in²ZX: Upright; ISO 180
 13.9 kJ/m²6.61 ft-lb/in²XY: Flat; ISO 180
 17.8 kJ/m²8.47 ft-lb/in²XZ: On its edge; ISO 180
Charpy Impact Unnotched 0.370 J/cm²1.76 ft-lb/in²ZX: Upright; ISO 179
 1.71 J/cm²8.14 ft-lb/in²XY: Flat; ISO 179
 1.89 J/cm²8.99 ft-lb/in²XZ: On its edge; ISO 179
Charpy Impact, Notched 0.180 J/cm²0.857 ft-lb/in²ZX: Upright; ISO 179
 0.610 J/cm²2.90 ft-lb/in²XY: Flat; ISO 179
 0.650 J/cm²3.09 ft-lb/in²XZ: On its edge; ISO 179
 
Thermal PropertiesMetricEnglishComments
Melting Point 259 °C498 °FISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 134 °C273 °FISO 75-2
Deflection Temperature at 1.8 MPa (264 psi) 124 °C255 °FISO 75-2
Glass Transition Temp, Tg 142 °C288 °FISO 11357-2
Flammability, UL94  V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
 V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
 
Processing PropertiesMetricEnglishComments
Processing Temperature 80.0 - 100 °C176 - 212 °FBed, Bed Material: PC adhesive
Nozzle Temperature 280 - 330 °C536 - 626 °F
Drying Temperature 100 °C212 °Fin a hot air dryer or vacuum oven
Dry Time 4.00 - 16.0 hour4.00 - 16.0 hour
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
Nozzle Diameter=0.6 mm
Print speed30-60 mm/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBASF3D019 / 312260

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.