Petrothene LB560201 is a high density polyethylene resin that exhibits good stiffness and environmental stress crack resistance. Typical applications include bottles for household chemicals such as bleach, cleaners and detergents. Applications: Bottles For Consumer Goods, Bottles for Industrial UseInformation provided by LyondellBasell. |