MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
CoorsTek CRB-100 Resin-Impregnated Carbon Graphite  (discontinued **)
Categories: Carbon; Graphite

Material Notes: General purpose CoorsTek CRB-100 material contains a chemically resistant resin offering performance in a wide range of media. This resin-impregnated carbon graphite provides friction and wear properties in pressed-to-size configurations for high-volume applications.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.80 g/ccASTM-C559-85
Porosity 1.0 %
Particle Size <= 101.6 µmGrain Size
 
Mechanical PropertiesOriginal ValueComments
Modulus of Elasticity 3100 ksiASTM-C747-74
Flexural Strength 83.0 MPa
Compressive Strength 207 MPaASTM-C695-81
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00180 ohm-cmASTM-C611-84
 
Thermal PropertiesOriginal ValueComments
CTE, linear 2.90 µin/in-°FASTM-C372
Thermal Conductivity 6.00 W/m-K
Maximum Service Temperature, Air 260 °C
 
Descriptive Properties
Hardness (Shore-Scleroscope)95

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow 734 FLOWABLE SEALANT
CoorsTek CRB-300 General-Duty Carbon Graphite
Graphite, Carbon, C
CoorsTek CRB-200 Resin-Impregnated Carbon Graphite
APCM DA 409U/G35 150 Unidirectional Carbon Epoxy Prepreg System

CCOOR904 / 104608

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.