MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ASI® MP531107I Acrylate Urethane UV-Curing Adhesive
Categories: Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes: MP531107I is a high performance UV curing adhesive engineered to bond plastics, metal, and glass. It can be used in a variety of product assemblies and it promotes innovative design solutions. It is a fast cure, strong bonding adhesive. Our MP531107I has passed ISO 10993 Cytotoxicity testing and is a leading performer when used for bonding general industrial applications. During in-line inspection this adhesive fluoresces a blue color when using a low intensity black light. MP531107I is often cured with an electroless lamp D, medium pressure metal halide lamp. This UV adhesive also works well with UV light emitted diodes (UV LED) at wavelengths of 365 nm to 410 nm. Design engineers select MP531107I for the optimum in finished product quality, reliability, performance, and cost effectiveness. MP531107I is an essential tool in improving overall product quality, lowering per unit cost, and reducing processing time. Benefits: Superior Bond Strength, Solvent Free, Low Odor, Improves Finished Product Quality, Durable, Good Impact and Vibration Resistance, Easily Automated, No Clean Up, Substrate Applications, PET, PVC, Polyethylene, Polypropylene requires surface treatment such as corona, etc., Metal, Glass.

Information provided by Adhesive Systems, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.02 g/cc0.0368 lb/in³uncured
Water Absorption  2.5 %
@Temperature 25.0 °C,
Time 86400 sec
2.5 %
@Temperature 77.0 °F,
Time 24.0 hour
cured
 3.0 %
@Temperature 100 °C,
Time 7200 sec
3.0 %
@Temperature 212 °F,
Time 2.00 hour
cured
Viscosity 180 - 270 cP
@Temperature 25.0 °C
180 - 270 cP
@Temperature 77.0 °F
20 rpm. Uncured
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7070
Tensile Strength 30.3 MPa4400 psi
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant <= 4.0<= 4.0cured
Dielectric Strength >= 15.7 kV/mm>= 400 kV/incured
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 149 °C300 °F
Minimum Service Temperature, Air -51.1 °C-60.0 °F
Glass Transition Temp, Tg 65.0 °C149 °Fcured
Flash Point 77.0 °C171 °Funcured
 
Descriptive Properties
Blue FluorescingYes. Cured
Chemical ClassAcrylate Urethane
Color / appearanceliquid
Flexible at Room Temperature?No

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PASINC9117 / 233484

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.