MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Teknor Apex Sinvicomp SSG 5003 Polyvinyl Chloride, Flexible
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Flexible Grade; PVC, Wire and Cable Grade

Material Notes: Availability: Asia Pacific

Features: Good Flexibility

Uses: Cable Jacketing; Wire and Cable Applications

Wire Types: ST4; ST5; TM1; YM1; YM2

Agency Ratings: BS 6746; IEC 60227; VDE 0207

Forms: Pellets

Processing Method: Extrusion

Information Provided by Teknor Apex

Key Words: PVC
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.48 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 83ASTM D2240
Tensile Strength, Yield 2223 psiAfter aging 168 hours at 176°F; ASTM D638
 2470 psi9.8 in/min; ASTM D638
Elongation at Break 240 %After Aging 168 hours at 176°F; ASTM D638
 300 %9.8 in/min; ASTM D638

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI 1016 Steel, cold drawn, 19-32 mm (0.75-1.25 in) round
AISI 1021 Steel, mock carburized at 910°C (1670°F) for 8 hours, 775°C (1430°F) reheat, water quenched, 175°C (350°F) temper, 25 mm (1 in.) round
AISI 1018 Steel, cold drawn, high temperature, stress relieved, 16-22 mm (0.625-0.875 in) round
The Chemical Company Methanol
Teknor Apex Sinvicomp SSG 6006 Polyvinyl Chloride, Flexible

PTEKNP158 / 129239

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.