MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Shin-Etsu Silicones SV-58000U High Strength Silicone Elastomer
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Silicone; Silicone Rubber

Material Notes: SV58000U is one of a series of silicone bases designed for applications requiring high strength.

Product Features:

  • Excellent mechanical properties.
Typical Applications:
  • Molding and Extrusion applications for a wide range of products

Information Provided by Shin-Etsu Silicones of America, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 79
Tensile Strength at Break 1422 psi
Elongation at Break 402 %
Tear Strength 125 pliDie B
Compression Set 23 %
@Temperature 177 °C,
Time 79200 sec
 
Processing PropertiesOriginal ValueComments
Cure Time 10.0 min
 
Descriptive Properties
Cure AgentDBPH
Cure TypePress Cure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Shin-Etsu Silicones KE-5006BU Low Temperature Silicone Elastomer
Shin-Etsu Silicones KE-5540U Low Temperature Silicone Elastomer
Shin-Etsu Silicones SV-18000U Silicone Rubber
Shin-Etsu Silicones KE-5550U Low Temperature Silicone Elastomer
Shin-Etsu Silicones KE-971TU Silicone Elastomer

PSHIN265 / 177776

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.