MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BASF Lupranate® 5090 Isocyanate
Categories: Fluid

Material Notes: Description: Lupranate® 5090 Isocyanate is a liquid prepolymer of pure, diphenylmethane diisocyanate (MDI). The Lupranate 5090 Isocyanate has been formulated for improved low-temperature stability compared to Lupranate MP102 Isocyanate. Lupranate 5090 Isocyanate has the potential to reduce handling and storage issues associated with field-applied, 2-component urethanes.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.19 g/cc
Viscosity 650 cP
Vapor Pressure 1.33e-8 bar
@Temperature 25.0 °C
 
Thermal PropertiesOriginal ValueComments
Boiling Point >= 190 °C
@Pressure 0.000667 MPa
Flash Point >= 200 °C
 
Descriptive Properties
ColorLight Yellow
CompositionHydrolyzable Chlorine<50.0%
 NCO content0.23

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
INEOS Styrolution Luran® S 776SE ASA
Bamberger Polymers Bapolene® 5090 Polypropylene Impact Copolymer Extrusion Grade
BASF Ultradur® B 4500 PBT
EMS-Grivory Grivory® HTV-4H1 black 9205 PA6T/6I-GF40
EMS-Grivory Grivory® HTV-4H1 nat PA6T/6I-GF40

PBASG0677 / 132310

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.