MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3M Scotch-Weld™ 5 Neoprene Contact Adhesive
Categories: Polymer; Adhesive

Material Notes: 3M™ Scotch-Weld™ Neoprene Contact Adhesive 5 is a sprayable contact adhesive which may be used to bond many high-pressure plastic laminates to wood, particle-board, metal and other surfaces

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 18 - 21 %18 - 21 %
Brookfield Viscosity 175 - 350 cP175 - 350 cPRVF #2 sp @ 20 rpm @ 80°F
 
Mechanical PropertiesMetricEnglishComments
Shear Strength  0.262 MPa
@Temperature 107 °C,
Time 1.81e+6 sec
38.0 psi
@Temperature 225 °F,
Time 504 hour
Overlap
 0.448 MPa
@Temperature 82.0 °C,
Time 1.81e+6 sec
65.0 psi
@Temperature 180 °F,
Time 504 hour
Overlap
 3.31 MPa
@Temperature 75.0 °C,
Time 1.21e+6 sec
480 psi
@Temperature 167 °F,
Time 336 hour
Overlap
 3.32 MPa
@Temperature 75.0 °C,
Time 1.81e+6 sec
482 psi
@Temperature 167 °F,
Time 504 hour
Overlap
 7.31 MPa
@Temperature -34.0 °C,
Time 1.81e+6 sec
1060 psi
@Temperature -29.2 °F,
Time 504 hour
Overlap
Peel Strength  1.23 kN/m
@Temperature 82.0 °C,
Time 1.81e+6 sec
7.00 pli
@Temperature 180 °F,
Time 504 hour
180°, Canvas/Steel
 1.75 kN/m
@Temperature 24.0 °C,
Time 86400 sec
10.0 pli
@Temperature 75.2 °F,
Time 24.0 hour
180°, Canvas/Steel
 2.10 kN/m
@Temperature 24.0 °C,
Time 259000 sec
12.0 pli
@Temperature 75.2 °F,
Time 72.0 hour
180°, Canvas/Steel
 2.45 kN/m
@Temperature 24.0 °C,
Time 432000 sec
14.0 pli
@Temperature 75.2 °F,
Time 120 hour
180°, Canvas/Steel
 2.89 kN/m
@Temperature -34.0 °C,
Time 1.81e+6 sec
16.5 pli
@Temperature -29.2 °F,
Time 504 hour
180°, Canvas/Steel
 3.16 kN/m
@Temperature 24.0 °C,
Time 605000 sec
18.0 pli
@Temperature 75.2 °F,
Time 168 hour
180°, Canvas/Steel
 3.16 kN/m
@Temperature 24.0 °C,
Time 1.21e+6 sec
18.0 pli
@Temperature 75.2 °F,
Time 336 hour
180°, Canvas/Steel
 3.33 kN/m
@Temperature 24.0 °C,
Time 1.81e+6 sec
19.0 pli
@Temperature 75.2 °F,
Time 504 hour
180°, Canvas/Steel
 
Thermal PropertiesMetricEnglishComments
Flash Point -25.0 °C-13.0 °FTCC
 
Descriptive Properties
AppearanceGreen, Light Yellow
BasePolychloroprene

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M Scotch-Weld™ 10 Neoprene Contact Adhesive
3M Scotch-Weld™ 2141 Neoprene Rubber & Gasket Adhesive
3M Scotch-Weld™ 1357-L Neoprene High Performance Contact Adhesive
3M Scotch-Weld™ 1357 Neoprene High Performance Contact Adhesive
3M Scotch-Weld™ 1300L Neoprene High Performance Rubber Gasket Adhesives

PMM34111 / 168858

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.