Description: Master Bond Polymer System EP3AOHT is an epoxy resin system for electrical potting, encapsulation, and bonding. It combines high physical strength, including resistance to abrasion, thermal shock and heat. It has good thermal conductivity, is inert to water and chemicals, with good electrical insulation characteristics. It has a service temperature range from - 60°F up to 400°F. Adhesion to both metallic and nonmetallic substrates is excellent. Master Bond Polymer System EP3AOHT offers the application convenience of a one component epoxy system which eliminates mixing and provides flexible cure schedules to best meet specific application requirements. It is 100% reactive and does not contain any solvents or diluents. Master Bond Polymer System EP3AOHT is supplied in the form of a light gray paste having a minimum storage stability of more than 3 months when stored at room temperature. Refrigeration greatly extends the storage stability of this epoxy to 6 months. Gel time and cure schedules depend on temperature. The gel time at 150°C is in the order of 90-100 seconds. The recommended cure time at 150°C is in the order of 10-15 minutes and at 125°C in the order of 20-25 minutes. Typical performance properties of the Master Bond Polymer System EP3AOHT are listed below.Information provided by MasterBond® |
Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.Click here to view all available suppliers for this material. Please click here if you are a supplier and would like information on how to add your listing to this material. |