MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Teknor Apex Sarlink® TPV X4145B-W1 BLACK Thermoplastic Vulcanizate
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: Notes: Sarlink X4145BW1 BLACK is a specially developed engineering material designed primarily for demanding consumer, industrial, and automotive applications. This product is a low density, medium hardness thermoplastic vulcanizate that exhibits excellent compression set, flex fatigue, high and low temperature performance and very good chemical resistance including copper contact. This grade can be processed by injection molding, extrusion, and profile extrusion.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: Chemical Resistant; Copper Contact Stabilized; Filled; Good Melt Strength; Good Processability; High Heat Resistance; Low Compression Set; Low Density; Low Specific Gravity; Medium Hardness; Resilient

Uses: Appliance Components; Automotive Applications; Bushings; Consumer Applications; Diaphragms; Gaskets; Industrial Applications; O-rings; Plugs; Profiles; Rubber Replacement; Seals; White Goods & Small Appliances

RoHS Compliance: RoHS Compliant

Agency Ratings: UL 94

UL File Number: QMFZ2.E54709

Form: Pellets

Processing Method: Injection Molding; Extrusion; Profile Extrusion

Preliminary data. Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.960 g/ccISO 1183
Viscosity 323 cP
@Shear Rate 206 1/s,
Temperature 200 °C
Apparent; ASTM D3835
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 45
@Time 5.00 sec
Extruded; ISO 868
 48
@Time 5.00 sec
Injection Molded; ISO 868
Tensile Strength at Break 595 psiAcross Flow; ISO 37
Tensile Stress at Strain 203 psi
@Strain 100 %
Across Flow; ISO 37
Elongation at Break 500 %Across Flow; ISO 37
Tear Strength 110 pliMethod Ba, Angle (Unnicked); ISO 34-1
Compression Set 14 %
@Temperature 22.8 °C,
Time 79200 sec
ISO 815
 27 %
@Temperature 70.0 °C,
Time 79200 sec
ISO 815
 
Processing PropertiesOriginal ValueComments
Processing Temperature 360 - 430 °FInjection, Melt
Rear Barrel Temperature 350 - 420 °FInjection
Middle Barrel Temperature 350 - 420 °FInjection
Front Barrel Temperature 350 - 420 °FInjection
Nozzle Temperature 370 - 430 °FInjection
Zone 1 360 - 400 °FExtrusion
Zone 2 360 - 400 °FExtrusion
Zone 3 370 - 410 °FExtrusion
Zone 4 370 - 410 °FExtrusion
Die Temperature 380 - 420 °FExtrusion
Melt Temperature 380 - 420 °FExtrusion
Mold Temperature 50.0 - 150 °FInjection
Drying Temperature 180 °F
Dry Time 3.00 hour
Back Pressure 10.0 - 150 psiInjection
Screw Speed 100 - 200 rpmInjection
 
Descriptive Properties
AppearanceBlack
 Opaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTEKNQ1204 / 237695

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.