MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Lanxess LEWATIT® S 2568 H Cation Exchange Resin
Categories: Polymer; Thermoset

Material Notes: Lewatit® S 2568 H is a food grade, macroporous, monodisperse, strongly acidic cation exchange resin based on a styrene-divinylbenzene copolymer. Lewatit S 2568 H is especially applicable for:
  • the decationization of solutions of organic products, e.g. sugar beet, sugar cane, starch sugar, glycerin, gelatin, whey and food acids etc.
  • the extraction of amino acids e.g. lysine
  • mixed bed polishing
Lewatit S 2568 H is adding special features to the resin bed:
  • high exchange flow rates during regeneration and loading
  • a good utilization of the capacity, low rinse water demand
  • a homogenous throughput of regenerants, water and solutions; therefore a homogeneous working zone
  • a nearly linear pressure drop gradient for the whole bed depth; therefore an operation with higher bed depth possible
  • a good separation behavior of the components in a mixed bed application
If using Lewatit S 2568 H to treat potable water and the aqueous solutions listed above, special care should be given to the initial cycles of the new resin.

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.740 g/cc
Density 1.18 g/cc
Bead Size 0.620 - 0.720 mmMean
Storage Temperature -20.0 - 40.0 °C
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 120 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life 24.0 Month
 
Descriptive Properties
AppearanceBeige-grey, opaque
pH Operating Range0 - 14

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLANY8824 / 209216

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.