MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
Ensinger TECASON™ S Polysulfone (PSU)
Categories: Polymer; Thermoplastic; Polysulfone (PSU)

Material Notes: TECASON™ S is a transparent engineering plastic known for its chemical resistance, rigidity, high-temperature performance, and its ability to operate in an autoclave environment. TECASON™ S is FDA and NSF compliant and holds its excellent mechanical properties over a wide range of temperatures.

  • Autoclave resistance (maintains dimensional stability and mechanical performance through repeated autoclaves)
  • Excellent electrical properties
  • Good chemical resistance (performs well in mineral acids, alkali, salt solutions, and hydrocarbons)
  • Superior resistance to creep
  • FDA and NSF compliant
  • High-temperature performance (has a heat deflection temperature of 345°F and a long-term continuous use temperature of 285°F)
  • Excellent hydrolytic stability
  • High strength and rigidity
  • Flame retardant (rated UL94 V-O)

TECASON™ S' unique combination of chemical and hydrolytic resistance, high-temperature performance, good mechanical properties, and agency approvals make it an excellent choice for applications in pharmaceutical, medical, food service equipment, semiconductor processing, and electronic equipment industries.

Information Provided by Ensinger Industries, Inc.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.24 g/ccASTM D792
Density 0.0450 lb/in³ASTM D792
Water Absorption 0.30 %
@Temperature 22.8 °C,
Time 86400 sec
ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 120ASTM D785
Tensile Strength at Break 10200 psi
@Temperature 22.8 °C
ASTM D638
Elongation at Break >= 100 %
@Temperature 22.8 °C
ASTM D638
Tensile Modulus 360000 psi
@Temperature 22.8 °C
ASTM D638
Flexural Strength 15400 psi
@Temperature 22.8 °C
ASTM D790
Flexural Modulus 390000 psi
@Temperature 22.8 °C
ASTM D790
Izod Impact, Notched 1.30 ft-lb/in
@Temperature 22.8 °C
ASTM D256
Coefficient of Friction, Dynamic 0.37
@Pressure 0.276 MPa
50 fpm
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 5.00e+16 ohm-cm
@Temperature 22.8 °C
ASTM D257
Dielectric Constant 3.1
@Frequency 60 Hz,
Temperature 22.8 °C
50% RH; ASTM D150
Dielectric Strength 425 V/milASTM D149
Dissipation Factor 0.0010
@Frequency 60 Hz,
Temperature 22.8 °C
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 31.0 µin/in-°FASTM D696
Maximum Service Temperature, Air 285 °FLong Term
 340 °FShort Term
Deflection Temperature at 0.46 MPa (66 psi) 358 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 345 °FASTM D648
Vicat Softening Point 371 °F
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90 %transparent; thickness not quantified

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Avient Edgetek® PF-20GF/000 Polysulfone (PSU)
BASF Ultrason® S 2010 G6 30% Glass Filled PSU
BASF Ultrason® S 2010 PSU
BASF Ultrason® S 2010 G4 20% Glass Filled PSU
Ensinger TECAPRO™ SAN Polypropylene (PP)

PENSIN029 / 92846

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.