Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
GS Caltex HI-PRENE H551 PP, Homopolymer
Categories:
Polymer
;
Thermoplastic
;
Polypropylene (PP)
Material Notes:
Product features: Excellent stiffness and slip property
Final product: Food containers, disposable syringe components
Information provided by GS Caltex Corporation
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
0.900
g/cc
0.0325
lb/in³
ASTM D792
0.900
g/cc
0.0325
lb/in³
ISO 1183
Melt Flow
11
g/10 min
@Load 2.16 kg,
Temperature 230 °C
11
g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
11
g/10 min
@Load 2.16 kg,
Temperature 230 °C
11
g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties
Metric
English
Comments
Hardness, Rockwell R
105
105
ASTM D785
105
105
ISO 2039
Tensile Strength
35.0
MPa
5080
psi
ISO 527
37.0
MPa
5370
psi
ASTM D638
Elongation at Break
>= 500 %
>= 500 %
ASTM D638
>= 500 %
>= 500 %
ISO 527
Flexural Modulus
1.55
GPa
225
ksi
ISO 178
1.60
GPa
232
ksi
ASTM D790
Izod Impact, Notched
0.350
J/cm
0.656
ft-lb/in
ASTM D256
Izod Impact, Notched (ISO)
3.50
kJ/m²
1.67
ft-lb/in²
ISO 180
Thermal Properties
Metric
English
Comments
Deflection Temperature at 0.46 MPa (66 psi)
90.0
°C
194
°F
ISO 75
115
°C
239
°F
ASTM D648
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
PGSCAL051 / 294925
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.