MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Go Yen Chemical Goyenchem-GPPS25 General Purpose Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS)

Material Notes: Characteristic:
  • High Flow Grade
  • TPR compounding
Applications: TPR compounding, masterbatch

Information provided by Go Yen Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³ASTM D792
Melt Flow >= 20 g/10 min
@Load 5.00 kg,
Temperature 200 °C
>= 20 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 120120ASTM D785
Tensile Strength, Yield 37.3 MPa
@Thickness 3.17 mm
5410 psi
@Thickness 0.125 in
ASTM D638
Elongation at Break 2.0 %
@Thickness 3.17 mm
2.0 %
@Thickness 0.125 in
ASTM D638
Flexural Yield Strength 58.8 MPa
@Load 1.00 kg,
Thickness 3.00 mm
8530 psi
@Load 2.20 lb,
Thickness 0.118 in
120°C/h; ASTM D790
Flexural Modulus 2.94 GPa
@Load 1.00 kg,
Thickness 3.00 mm
426 ksi
@Load 2.20 lb,
Thickness 0.118 in
120°C/h; ASTM D790
Izod Impact, Notched 0.127 J/cm0.238 ft-lb/inA method, 1/4”×1/2”×5/2”; ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 77.0 °C
@Thickness 12.7 mm
171 °F
@Thickness 0.500 in
Unannealed; ASTM D648
Vicat Softening Point 85.0 °C
@Load 1.00 kg,
Thickness 3.00 mm
185 °F
@Load 2.20 lb,
Thickness 0.118 in
120°C/h; ASTM D1525
 
Processing PropertiesMetricEnglishComments
Processing Temperature 160 - 280 °C320 - 536 °FCylinder
Mold Temperature 35.0 - 65.0 °C95.0 - 149 °F
Injection Pressure 49.0 - 137 MPa7110 - 19900 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGOYEN787 / 267095

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.