MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Poco Graphite ACF-100Q Specialty Graphite  (discontinued **)
Categories: Carbon; Graphite

Material Notes: SSH hardness is 95.

General Poco Specialty Graphite Information: Poco's high strength, fine-grained, isotropic graphites offer maximum design flexibility. Easily machined. High strength and small particle size allow fabrication of complex components containing tight tolerances. Post synthesis treatments available include purification or impregnation with resins, oxidation inhibitors, or metals. Surface treatments offer improved wear characteristics and particle reduction.

Some applications of Poco specialty graphites include anode plates for wet cells, fuel cell plates for solid polymer cells, air bearings, hot gas valves, high temperature bearings, bushings, and seals, hot press dies and rams, furnace furniture/fixturing, rocket engine nozzles, molten metal casting components, vacuum furnace heating elements, space vehicle nose cones, mirrors and optical structures, and satellite heat shields.

Information provided by Poco Graphite, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Apparent Bulk Density 1.77 g/cc0.0639 lb/in³
Open Porosity 15 %15 %
Porosity 21 %21 %total porosity
Particle Size 5.0 µm5.0 µm
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 70.0 MPa10200 psi
Elongation at Break 0.62 %0.62 %
Modulus of Elasticity 11.0 GPa1600 ksi
Flexural Strength 95.0 MPa13800 psi
Compressive Yield Strength 185 MPa26800 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00246 ohm-cm0.00246 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 7.60 µm/m-°C
@Temperature 20.0 °C
4.22 µin/in-°F
@Temperature 68.0 °F
Thermal Conductivity 60.0 W/m-K416 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 470 °C878 °FOxidation threshold

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Graphite, Carbon, C
Carlisle 201HL Carbon-Carbon Composite
Aremco Graphi-Bond™ 551-R
Aremco Graphi-Bond™ 551-RN High Temperature Ceramic Adhesive/Paste, Graphite Filled
Aremco Graphi-Bond™ 669 High Temperature Ceramic Adhesive/Paste, Graphite Filled

EPOC01 / 5668

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.