MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
Ensinger Delrin® 150 Homopolymer Acetal (POM)
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Homopolymer, Unreinforced

Material Notes: Ensinger's Delrin® 150 stock shapes are a homopolymer acetal manufactured using DuPont Delrin 150 Resin. It is a crystalline plastic which offers an excellent balance of properties to bridge the gap between metals and plastics. It possesses high tensile and flexural properties, along with creep resistance and toughness, while exhibiting low moisture absorption, and fatigue endurance.

Information Provided by Ensinger, Inc.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.42 g/ccASTM D792
Water Absorption 0.25 %
@Time 86400 sec
ASTM D570
Water Absorption at Saturation 0.90 %ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 94ASTM D785
Hardness, Rockwell R 120ASTM D785
Tensile Strength, Yield 11000 psiASTM D638
Elongation at Break 25 %ASTM D638
Tensile Modulus 450000 psiASTM D638
Flexural Strength 16000 psiASTM D790
Flexural Modulus 420000 psiASTM D790
Compressive Strength 5200 psiASTM D695
Izod Impact, Unnotched 1.5 ft-lb/inASTM D256
Coefficient of Friction, Dynamic 0.2040 psi, 50 fpm; ASTM D3702
K (wear) Factor 55.0 x 10-10 in³-min/ft-lb-hrASTM D3702
Limiting Pressure Velocity 0.0513 MPa-m/secASTM D792
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmASTM D257
Dielectric Constant 3.7
@Frequency 60 Hz
50% RH; ASTM D150
Dielectric Strength 500 V/milASTM D149
Dissipation Factor 0.0050
@Frequency 60 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 68.0 µin/in-°FASTM D696
Melting Point 347 °FASTM D2133
Maximum Service Temperature, Air 185 °FContinuous; UL746B
 300 °FIntermittent
Deflection Temperature at 0.46 MPa (66 psi) 336 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 257 °FASTM D648
Flammability, UL94 HBUL 94

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Delrin Delrin® 150 NC010 POM
Overview of materials for Acetal Copolymer, Unreinforced
Ensinger DELRIN® 100AF Acetal Homopolymer, 13% PTFE filled (POM)
Ensinger DELRIN® 507 Black Acetal Homopolymer (POM)
Overview of materials for Acetal Homopolymer, Unreinforced

PENSIN065 / 104756

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.