MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
CIMBAR Crescent 35 Calcium Carbonate (CaCO3), Medium Powder
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: CIMBAR's Crescent product line is a natural calcium carbonate ground to various particle size distributions. The crystalline structure of the calcium carbonate in Crescent products has a predominantly spherical shape, and is essentially crystalline silica-free (less than 0.1%). These properties promote low abrasion to mixing and extrusion equipment while enhancing extrusion rates and overall productivity.

Applications:

  • Resins
  • PVC
  • Polyolefins
  • Paints and Coatings
  • Polyurethane
  • Putties
  • Rubber Compounds
  • Mastics
  • Patching Compounds
  • Tile Grouts/Caulks
  • Adhesives and Sealants
  • Drilling fluid/Oil field applications

Information provided by Cimbar Performance Minerals.

Key Words: CaCO3
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Particle Size 16 - 24 µmFor Median
 20 µmTarget Median Particle Size
Particle Mesh Size 200 Mesh65% passing, wet
 
Component Elements PropertiesOriginal ValueComments
Al2O3 0.18 %
Fe2O3 0.080 %
MgO 0.0040 %
SiO2 0.20 %
 
Descriptive Properties
Acid Solubility98.00 Min.
CaCO393Min
 97.82Typical
MgCO31.27

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
CIMBAR Crescent 12 Calcium Carbonate (CaCO3), Fine Powder
CIMBAR RiverCal™ 8107 & 8107C Calcium Carbonate (CaCO3)
Calcium Carbonate, Calcite (CaCO3)
CIMBAR Crescent 50 Calcium Carbonate (CaCO3), Coarse Powder
Excalibar ExCal® 200 Calcium Carbonate CaCO3 Powder

CIMBAR949 / 133431

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.